Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 177 - 191 °C | 350 - 375 °F | Recommended Stock Temperature |
Sylvin Technologies 5748 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 177 - 191 °C | 350 - 375 °F | Recommended Stock Temperature |
Sylvin Technologies 6046 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 157 - 191 °C | 315 - 375 °F | Average value: 174 °C Grade Count:46 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |