Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Plasticizing Zone |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Plasticizing Zone |
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring .. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Plasticizing Zone |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | Mixture Zone; Coextrusion with polyamide |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Molding temperature |
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | thermoforming temperature |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Profiles and hoses |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Blow molding |
Lucobit Lucofin® 1400MN Ethylene Butyl Acrylate Lucofin 1400MN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400MN is softer and more flexible than ethylene homopoly.. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Blown film |
Lucobit Lucofin® 1400SL Ethylene Butyl Acrylate Lucofin® 1400SL is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin® 1400SL is softer and more flexible than ethylene h.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A7551E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8760F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8910K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® A8915K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | |
Taiwan Sheen Soon Sheenthane® AH-585K Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmHotmelt adhesive gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-785A TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-975B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-980 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem MP-855WR TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 175 - 190 °C | 347 - 374 °F | |
Wanhua Chemical Wanthane® WHT-8180 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | |
Wanhua Chemical Wanthane® WHT-A880 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 150 - 190 °C | 302 - 374 °F | Films Die Head |
EMS-Griltech Griltex® D 1556A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | |
Fainplast Compounds EVAtech 801S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Processing Temperature | 180 - 190 °C | 356 - 374 °F | |
Fainplast Compounds EVAtech 805S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Processing Temperature | 160 - 190 °C | 320 - 374 °F | Blown film |
Lucobit Lucofin® 1400HN Ethylene Butyl Acrylate Lucofin 1400HN is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN is softer and more flexible than ethylene homopolym.. |