Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 721 - 816 °C | 1330 - 1500 °F | Brazing Range |
Lucas-Milhaupt BRAZE 380 Characteristics:Braze 380 is a free-flowing, low temperature filler metal with excellent wetting of most ferrous and non-ferrous base metals, and is a good substitute for cadmium-bearing filler meta.. |
|||
Processing Temperature | 680.0 - 816 °C | 1256 - 1500 °F | Brazing Range |
Lucas-Milhaupt BRAZE 452 Characteristics:Braze 452 is a free-flowing, low temperature filler metal commonly used to replace cadmium-bearing filler metals of similar silver content. This alloy is best suited for narrow gap .. |
|||
Processing Temperature | 699 - 816 °C | 1290 - 1500 °F | Brazing Range |
Lucas-Milhaupt BRAZE 495 Carbide Brazing Alloy Applications: Because of its excellent wetting properties, Braze 495 is used extensively for brazing tungsten carbide inserts to cutting tools and rock drills. It may be used for joining all types .. |
|||
Processing Temperature | 704 - 816 °C | 1300 - 1500 °F | Brazing Range |
Lucas-Milhaupt SIL-FOS 2 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 2 is a low cost brazing filler metal suitable for joining copper to copper and copper to copper alloys where critical impact or vibration stresses are not encountered in servi.. |
|||
Processing Temperature | 704 - 816 °C | 1300 - 1500 °F | Brazing Range |
Lucas-Milhaupt SIL-FOS 5 Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos 5 was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditionin.. |
|||
Processing Temperature | 704 - 816 °C | 1300 - 1500 °F | Brazing Range |
Lucas-Milhaupt SIL-FOS Silver/ Copper/ Phosphorus Alloy Applications: Sil-Fos was developed primarily for use on copper, but their use has extended to other nonferrous copper base alloys. It is used extensively on refrigeration units, air conditioning .. |
|||
Processing Temperature | 718.3 - 816 °C | 1325 - 1500 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 5 Brazing Alloy Silvaloy 5 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It is primarily used for the joining of copper-to-copper on .. |
|||
Processing Temperature | 688 - 816 °C | 1270 - 1500 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 50N Brazing Alloy Silvaloy 50N is a modification of Silvaloy 50. It was originally introduced because of somewhat better corrosion resistance than Silvaloy 50 for certain conditions, and is still used for such purpos.. |
|||
Processing Temperature | 718.3 - 816 °C | 1325 - 1500 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 6 Brazing Alloy Silvaloy 6 is used for the brazing of copper and copper alloys, brass and bronze. It can also be used on silver, tungsten and molybdenum. It should not be used on ferrous and nickel metals or copper.. |
|||
Processing Temperature | 704 - 816 °C | 1300 - 1500 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 15 Brazing Alloy Silvaloy 15 is used for the brazing of copper and copper alloys, brass, and bronze. It can also be used on silver, tungsten and molybdenum. It is very effective for joining pipe and tubing and is wi.. |