Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 505 °C | 941 °F | Solution Heat Treatment |
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi.. |
|||
Processing Temperature | 505 °C | 941 °F | Solution Heat Treatment |
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us.. |