Polymer Property : Processing Temperature = 69.8 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Henkel Alodine T 5900 RTU Conversion Coating
Alodine T 5900 RTU treatment is a complex trivalent chromium conversion coating formulated for treating aluminum and its alloys, metals coated with IVD aluminum, magnesium, titanium and zinc surface..
Processing Temperature 21.0 - 71.0 °C
69.8 - 160 °F
Henkel Turco Metal Glo FF Jet Metal Brightener
Turco Metal Glo FF is a nonflammable, non-fluoride, acid based cleaner, brightener, deoxidizer and prepaint conditioner for aluminum. Turco Metal Glo FF contains viscosity builders that allow for ad..
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Henkel Alodine 1000L (Liquid) Conversion Coating
Alodine 1000L is a liquid chemical used to produce a protective coating on aluminum and aluminum alloys. The coating provides protection for aluminum and an excellent bond for organic coatings. Alod..
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Henkel Alodine 5700 Conversion Coating
Alodine 5700 is a chromium-free conversion coating specifically formulated for treating aluminum and its alloys. This product is formulated as a Ready-to-Use material for spray applications. The pro..
Processing Temperature 21.0 - 38.0 °C
69.8 - 100 °F
Henkel Turco Metal Glo #6 Jet Metal Brightener
Turco Metal Glo #6 is a nonflammable, tri-acid, detergent-solvent based cleaner, brightener, deoxidizer and prepaint conditioner for aluminum. It contains viscosity builders that allow for added con..
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Henkel Alodine T 5900 Conversion Coating
Alodine T 5900 treatment is a complex trivalent chromium conversion coating formulated for treating aluminum and its alloys, metals coated with IVD aluminum, magnesium, titanium and zinc surfaces. T..
Processing Temperature 21.0 - 32.0 °C
69.8 - 89.6 °F
Henkel Alodine T 5923 Conversion Coating
Alodine T 5923 treatment is a complex trivalent chromium conversion coating formulated for treating aluminum and its alloys, metals coated with IVD aluminum, magnesium, titanium and zinc surfaces. T..