Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 340 - 400 °C | 644 - 752 °F | Hardening Temperature |
Möller Medical TafSkin 103 NanoCoating Highly flexible, non-abrasive, chemical-resistant PTFE coating with very good easy-to-clean properties, biocompatible.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 340 - 400 °C | 644 - 752 °F | Hardening Temperature |
Möller Medical TafSkin 109 L NanoCoating Electrically conducting, chemical-resistant, thin, easy-to-clean PTFE coatingInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 340 °C | 644 °F | |
Shinil Chemical SHINCON PEI-CNT Magazine Rack Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp.. |
|||
Processing Temperature | 340 °C | 644 °F | |
Shinil Chemical SHINCON PES-CNT Magazine Rack Magazine Rack is used to transfer, handle, and bake lead frame or PCB substrate in semiconductor and LED packaging assembly process. Current Metal Magazine is made of anodized aluminum which is exp.. |