Polymer Property : Processing Temperature = 599 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 315 - 340 °C
599 - 644 °F
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Processing Temperature <= 315 °C
<= 599 °F
DuPont™ Appeel® 45D747 Polyolefin
Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion..
Processing Temperature 315 °C
599 °F
Extrusion Coating
Westlake EMAC® SP 1205 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
20% Methyl Acrylate Content. Characteristics: Processing Temperature Range: 280-600°F, Less Crystalline and Softer than Polyethylene, Excellent Thermal Stability Allows Extrusion Processing up to ..
Processing Temperature 315 °C
599 °F
Extrusion Coating
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows ..