Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 293 °C | 560 °F | |
Oxford Polymers 40GF 40% Glass Fiber Filled Polycarbonate for Injection Molding 40% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 293 - 304 °C | 560 - 580 °F | |
Oxford Polymers Oxnilon 66-50GF 50% Glass Fiber Filled Nylon 66 for Injection Molding 50% Glass Fiber Filled Nylon 66 for Injection MoldingInformation provided by Oxford Polymers. |
|||
Processing Temperature | 293 - 321 °C | 560 - 610 °F | Average value: 307 °C Grade Count:4 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Processing Temperature | 293 - 321 °C | 560 - 610 °F | Average value: 309 °C Grade Count:3 |
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma.. |
|||
Processing Temperature | 293 °C | 560 °F | |
Oxford Polymers 20GF 20% Glass Fiber Filled Polycarbonate for Injection Molding 20% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |