Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-8019 PPO, with glass fiber and PTFE, low-warpage Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour... |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1800-8435 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 6100 Flame Retardant PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1700-1401 PPO, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1800-7432 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | 280 °C | 536 °F | mass temp |
Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 2100 LT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Kingfa LONOY 2200 HT PC/PET Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Processing Temperature | 280 °C | 536 °F | maximum surface temperature, curing tube |
Borealis LE0516 Polyethylene Compound, Crosslinkable, Semiconductive LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive s.. |
|||
Processing Temperature | 280 - 320 °C | 536 - 608 °F | Recommended for injection molding. |
DuPont Selar® PA 3426 Nylon Barrier Resin Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural pro.. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA210GM , GF/MF Reinforced PA66, DAM GF/MF reinforced, Heat resistance, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM 15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
E-Polymers TEKAMID® TA250G45 , 45% Glass Fiber Reinforced PA66, DAM 45% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-MAX® AS 38 Anti-static masterbatch, LLDPE based Fields of application: Anti-static masterbatch for olefinicsExamples: Thermoformed and injection molded PP or PE products such as containers and other packaging products. Other applications are film.. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp ADD-VANCE® AS 884 Anti-static masterbatch, PP based Fields of application: Anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications.. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | Resin Temperature |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Dry as Molded Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Processing Temperature | 280 - 310 °C | 536 - 590 °F | Melt |
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. .. |
|||
Processing Temperature | <= 280 °C | <= 536 °F | |
Addcomp PRIEX® 20097 Maleic Anhydride Grafted PP homopolymer Fields of application: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fibre, wood flour, natural fibres, multilayer films, aluminium foils, .. |
|||
Processing Temperature | 280 - 315 °C | 536 - 599 °F | Injection Temp. |
Beijing Chemical Industry KAIFA® S-114 PPS Resin Glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 280 - 315 °C | 536 - 599 °F | Injection Temp. |
Beijing Chemical Industry KAIFA® S-206 PPS Resin Glass fiber reinforced and mineral filledInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Processing Temperature | 280 °C | 536 °F | See Materials Notes |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Processing Temperature | 280 °C | 536 °F | See Materials Notes |
BASF Capron® 8351 Impact Modified Nylon 6 (Conditioned)
(discontinued **) Capron 8351 is a type 6 polyamide graft copolymer developed for injection molding applications requiring a high level of toughness combined with moderate flexibility and faster cycles. It is also .. |
|||
Processing Temperature | 280 - 300 °C | 536 - 572 °F | |
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM Beautiful surface, strength propertyInformation provided by E-Polymers Co. Ltd. |