Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529 High Temperature Specialty Coatings Silicone Transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4090 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating This advanced silicon carbide, water-based coating reduces significantly the oxidation of graphite and carbon components and structures at temperatures to 2550 °F (1400 °C). Provides a hard surfac.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95% This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for se.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C) |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass Glass coating for producing hermetic seals in porous ceramics and refractories to 1450 ºF. Used for sealing high vacuum components, resistance temperature devices, and other electrical sensors. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, matte silver coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, white coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadi.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4040 High Temperature Protective Coating Silicone Low viscosity, white coating for motor windings to 1100°F (593°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating This pure, alumina based compound creates a hard, high temperature resistant coating for refractory fiber boards and shapes, providing exceptional resistance to molten metals and open flames to 3200.. |
|||
Processing Temperature | 10.0 - 32.2 °C | 50.0 - 90.0 °F | Application Temperature |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |