Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of aut.. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 170 - 180 °C | 338 - 356 °F | Collar Temperature |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® SMT-B-1™ Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA). It is formulated with a unique resin system that min.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
Processing Temperature | 170 - 185 °C | 338 - 365 °F | Molding temperature |
Cookson Group Plaskon® 150.401 Encapsulation Resin
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A second generation SMT-B family product. This material is the initial developmental, general purpose SMT-B encapsulation grade .. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Schedule: 5/20 min @ 170/220°C |
Huntsman HT 3380-1 Special Hardener Mix Ratio with GT 7013 is 18.Comments/Applications: Acid-anhydride functional crosslinker useful in FDA powder and can coating applications. *Mix ratio with GT 7013.Data provided by Ciba Specialty.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Schedule: 5/20 min @ 170/220°C |
Huntsman HZ 3365 Special Hardener Mix Ratio with 100 phr GT 6097 or GT 6609 US is 25.Comments/Applications: Hardener in solution for heat curing systems useful in can and coil applications. *Mix ratio with GT 6097 or GT 6609 US.Da.. |
|||
Processing Temperature | 170 - 250 °C | 338 - 482 °F | |
IRPC Polimaxx Polene 2500H Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT HIGH IMPACT, HIGH TOUGHNESS GOOD EXTRUDABILITYAPPLICATIONS: SHEET / BLOW MOLD EXTRUSION AND INJECTION MOLDING FOR CORRUGATE SHEETS, SHEETS FOR FILE, HOUSEWARES, CONTAINERS.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | |
IRPC Polimaxx Polene GM2865 High Density Polyethylene CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem GP-950 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 190 °C | 338 - 374 °F | Metering Temperature, Extrusion |
Stellarchem LP-870 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 170 - 230 °C | 338 - 446 °F | |
Zhejiang Juner PP6-1JE PP For Automotive Parts Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | Extrusion |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 400501S SBS Based Material, 50A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 420501S SBS Based Material, 50D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 210 °C | 338 - 410 °F | |
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Processing Temperature | 170 - 200 °C | 338 - 392 °F | Films Die Head |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | |
Cyclics CBT® 200 Thermoplastic Resin CBT® 200 resin melts to a water-like viscosity when heated, then polymerizes into the engineering thermoplastic resin polybutylene terephthalate (PBT). CBT 200 resin has a processing range between.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-621 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: General purpose with excellent sol.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-723 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Excellent mold releasability, non-sticking.Information provided by Dai.. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-752 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Information provided by Daikin Industries. |
|||
Processing Temperature | 170 °C | 338 °F | Cure Measuring Temperature |
Daikin DAI-EL G-783 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Fast vulcanization, for complex shapes.Information provided by Daikin .. |
|||
Processing Temperature | 170 - 240 °C | 338 - 464 °F | Injection molding |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |