Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 165 °C | 329 °F | Cure Temp |
Multibase SILASTIC® 7-6860 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® CX 7020 LDPE - Cast Film The Trithene® CX 7020 resin is a low-density polyethylene (LDPE) with medium molecular weight, excellent processability, and low gel content. Those features allow a production of thin and highly un.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone; Monoextrusion |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Plasticizing Zone |
Petroquimica Triunfo Trithene® TS 7003 LDPE - High Strength Film The Trithene TS 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily proc.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone; Monoextrusion |
Petroquimica Triunfo Trithene® TS 7006 LDPE - Coextruded Film The Trithene TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and strength.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Processing Temperature | 165 - 190 °C | 329 - 374 °F | Sheet Forming |
Polycasa SAN QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional s.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing .. |
|||
Processing Temperature | 165 - 180 °C | 329 - 356 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transpar.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Mixture Zone |
Petroquimica Triunfo Trithene® TX 8024 LDPE - High Clarity Film The Trithene TX 8024 resin is a low-density polyethylene (LDPE) with high molecular weight and distribution narrow, designed to obtain films with very high clarity and excellent processability. This.. |
|||
Processing Temperature | 165 - 175 °C | 329 - 347 °F | Molding temperature |
Cookson Group Plaskon® PPF-165A Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A conventional molding compound specifically formulated for semiconductor devices which are molded with preplated leadframes. Lo.. |
|||
Processing Temperature | <= 165 °C | <= 329 °F | Maximum Junction Temperature |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Processing Temperature | 165 - 200 °C | 329 - 392 °F | |
Taiwan Sheen Soon Sheenthane® A8800F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Processing Temperature | 165 - 250 °C | 329 - 482 °F | |
Zhejiang Juner JEPPA003 High Glossy PP Applications: High Glossy PartsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 165 °C | 329 °F | Cure 2 hrs |
Aptek 6500-PMF Electrically conductive epoxy adhesive High purity, low outgassing, electrically conductive adhesiveAPTEK 6500-PMF is a one component, pre-mixed frozen, 100% solid, silver-filled epoxy adhesive specifically designed for microelectronic d.. |