Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
KYDEX® V Acrylic/PC Thermoplastic Sheet Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 101 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Thermoplastic sheet for signageApplications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirableFeatures: Kydex 101 is more rigid than most o.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet
(discontinued **) USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may.. |
|||
Processing Temperature | 162 - 200 °C | 324 - 392 °F | Forming Temperature |
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd.. |