Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 143 - 287 °C | 289 - 549 °F | Injection |
Dyna-Purge® K Purging Compound Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow nat.. |
|||
Processing Temperature | 143 - 287 °C | 289 - 549 °F | Extrusion |
Dyna-Purge® K Purging Compound Designed or a broad range of "Low-Temp" resinsGeneral Description:DYNA-PURGE K is a low-temp, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow nat.. |
|||
Processing Temperature | 143 °C | 289 °F | |
Ashley Polymers Ashlene® ABS Resin R2018, 18% Glass Reinforced General purpose, 18% glass reinforced ABS resin.Data provided by the manufacturer |
|||
Processing Temperature | 143 - 160 °C | 289 - 320 °F | Average value: 156 °C Grade Count:4 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |