Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1020 °C | 1860 °F | fusing temperature |
Wall Colmonoy COLMONOY® 98 - Nickel-Based Alloy With Chromium Carbide Description and Application: Nickel-based alloy with superior resistance to corrosive liquids. Low coefficient of friction to reduce metal-to-metal adhesive wear loss.Method of Application: Spraywe.. |