Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 0024 Specialty Glass Glass Type: Si-B-MG-Al Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-ph.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 0026 Glaze and Sealant Glass Glass Type: Ca-B-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insul.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro EG 2778 Thick Film Glass Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
Processing Temperature | 899 - 954 °C | 1650 - 1750 °F | Brazing Range |
Lucas-Milhaupt Lucanex 716 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Processing Temperature | 899 - 1010 °C | 1650 - 1850 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® X55 Brazing Alloy Silvaloy X55 has excellent gap filling capability and plasticity when in the molten condition. It also exhibits excellent strength and ductility while cooling from the liquid stage. The improved str.. |
|||
Processing Temperature | 900 °C | 1650 °F | Typical Firing Temperature |
Ferro F 2719 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Kovar Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals.. |
|||
Processing Temperature | 899 - 954 °C | 1650 - 1750 °F | Brazing Range |
Lucas-Milhaupt Cerametil 716 Active Metal Brazing BR 716 strip coated with Ti for joining ceramics without metallization.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal strip in wrought Cerametil |
|||
Processing Temperature | 899 °C | 1650 °F | fusing temperature |
Wall Colmonoy COLMONOY® 225 - Custom Formulated Nickel-Based Alloy For Glass Description and Application: Patented alloy specially designed for glass container mold protection and restoration. Also used for rebuilding automotive parts (clutch components).Method of Applicati.. |