Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 710 °C | 1310 °F | Typical Firing Temperature; Typical Firing Time: 10-15 min. at Peak |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® A50N Flux Coated Rod Brazing Alloy Silvacote A50N Flux Cored is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel t.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy Silvacote A50N Flux Coated Rod is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nic.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvacote® A50N Brazing Alloy Silvacote A50N is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silve.. |
|||
Processing Temperature | 710 - 843 °C | 1310 - 1550 °F | Brazing Temperature |
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s.. |
|||
Processing Temperature | 710 °C | 1310 °F | Flow Temp |
Wieland Porta Oprimum 710 Solder Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental |