Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 45.0 - 249 °C | 113 - 480 °F | Average value: 171 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/05 Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: DIY, AutomotiveInformation provided by Merquinsa |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/11S Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/08 Polycaprolactone based TPU Pearlstick 45-40/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level. Solubility.. |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/27 Polycaprolactone based TPU Pearlstick 45-40/27 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility:.. |
|||
Processing Temperature | 45.0 °C | 113 °F | Roll 1 Temperature |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/15 Polycaprolactone based TPU Pearlstick 45-40/15 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level. Solubility: .. |
|||
Processing Temperature | 45.0 °C | 113 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-40/19 Polycaprolactone based TPU Pearlstick 45-40/19 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a medium thermoplasticity level.Solubility: P.. |