Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 25.0 - 80.0 °C | 77.0 - 176 °F | Hardening Temperature |
Möller Medical PolySkin 78 M NanoCoating Decorative coating in "metallic look," hardening at room temperature up to 80°C.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706D2 Polymer Dielectric This material is a cream colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode.. |
|||
Processing Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |
Gwent Electronic Materials D50706P3 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Processing Temperature | 65.0 - 80.0 °C @Time 900 sec |
149 - 176 °F @Time 0.250 hour |
|
Henkel Turco 5948-R Deoxidizer Turco 5948-R is an alkaline, water-based, blue, concentrated compound formulated to effectively clean painted and unpainted aircraft exterior and interior surfaces when diluted with water. Ideally s.. |
|||
Processing Temperature | 20.0 - 80.0 °C | 68.0 - 176 °F | Chill Roll |
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 6040 S01 is a second generation metallocene high density polyethylene.Lumicene® mPE M 6040 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excel.. |
|||
Processing Temperature | 70.0 - 80.0 °C @Time 3600 sec |
158 - 176 °F @Time 1.00 hour |
|
Henkel Turco 5668 Deoxidizer Turco 5668 is a diphase, liquid paint remover developed to remove resistant coatings, such as aluminized silicones, polyurethanes, acrylics, epoxies and chromated primers without using phenols, chro.. |
|||
Processing Temperature | 50.0 - 80.0 °C | 122 - 176 °F | |
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |
|||
Processing Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
Henkel Turco 6776-LO Paint Remover Turco 6776-LO environmentally advantaged paint remover is low-odor, thixotropic, developed for effective stripping of such resistant finishes as epoxies, epoxy primers, polyurethanes and similar cat.. |