Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 55.0 - 70.0 °C | 131 - 158 °F | Immersion |
Henkel Turco 6849 Cleaner Turco 6849 is a clear, aqueous alkaline degreaser formulated to remove shop soils, marking inks, COSMOLINE, grease and lube oils from ferrous and non-ferrous alloys. Offers both exceptional effectiv.. |
|||
Processing Temperature | 60.0 - 70.0 °C | 140 - 158 °F | |
Lucobit Lucosol® Bitumen Road Binder Lucosol is a solvent based bitumen road binder made out of selected bitumen qualities and hydrocarbon solventsInformation provided by Lucobit AG |