Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 49.0 - 60.0 °C @Time 900 sec |
120 - 140 °F @Time 0.250 hour |
Immersion |
Henkel Turco 4215 NC-LT Cleaner Turco 4215 NC-LT is a white granular mix developed for cleaning ferrous and nonferrous alloys by spray, immersion and ultrasonic methods at low temperatures. Ideal for cleaning fuel and hydraulic co.. |
|||
Processing Temperature | 23.0 - 60.0 °C @Time 540 sec |
73.4 - 140 °F @Time 0.150 hour |
|
Henkel Turco 4409 Jet Engine Cleaner Turco 4409 is a clear, colorless liquid acid cleaner and deoxidizer designed for use on ferrous and non-ferrous alloys by immersion, spray and hand wipe methods. It is not intended for use on magnes.. |
|||
Processing Temperature | 38.0 - 60.0 °C @Time 900 sec |
100 - 140 °F @Time 0.250 hour |
Immersion |
Henkel Turco Liquid Sprayeze NP-LT Cleaner Turco Liquid Sprayeze NP-LT is a straw-colored liquid, developed to remove shop soil, lube oils, light drawing oils and drawing waxes from ferrous, aluminum, copper and titanium alloys. In addition,.. |
|||
Processing Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Chill Roll |
Total Lumicene® mPE M 4040 Metallocene Polyethylene, Cast Film Lumicene® mPE M 4040 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 4040 can be processed at high output rates with low extrusion pressure, low neck-in, ex.. |
|||
Processing Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Chill Roll |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Processing Temperature | 50.0 - 60.0 °C | 122 - 140 °F | Tacking Temperature |
Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Processing Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Chill Roll |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |
|||
Processing Temperature | 21.1 - 60.0 °C | 70.0 - 140 °F | Average value: 28.9 °C Grade Count:14 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |