Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 288 - 321 °C | 550 - 610 °F | Average value: 304 °C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Processing Temperature | 293 - 321 °C | 560 - 610 °F | Average value: 308 °C Grade Count:13 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |