Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 121 - 154 °C | 250 - 309 °F | Thermoforming |
OCTAL DPET™ PET Sheet Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechan.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 309 °F | Thermoforming |
OCTAL DPET™/PE Lock-Up Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Processing Temperature | 121 - 154 °C | 250 - 309 °F | Thermoforming |
OCTAL DPET™/PE Peelable Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,.. |
|||
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |
|||
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 310 °F | Thermoforming Temp |
Alcoa KAMA 4100 Prime APET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Available in clear,.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 310 °F | Thermoforming Temp |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 310 °F | Thermoforming Temp |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1200 Utility Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1500 Freezer Modified OPS
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 310 °F | Thermoforming Temp |
Alcoa KAMA 4203 Impact Modified RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Processing Temperature | 121 - 154 °C | 250 - 310 °F | Thermoforming Temp |
Alcoa KAMA SealPET™ 4205 RF Sealable RPET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Silicone coating a.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |