Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 300 °C | <= 572 °F | |
Nabaltec APYMAG® 40 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Nabaltec APYMAG® 80 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Nabaltec APYMAG® 80S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PA1501 Polyamide 66 - Carbon Nanotube Masterbatch PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | 300 °C | 572 °F | Material Temperature |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 3 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
PolyChem Alloy PolySept 101M PolySept products typically contain 5 – 20% of an antimicrobial agent that is compounded into a plastic resin. The result is an antimicrobial polymer concentrate in a uniform pelletized form. PolyS.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
PolyChem Alloy PolySept 1007M PolySept products typically contain 5 – 20% of an antimicrobial agent that is compounded into a plastic resin. The result is an antimicrobial polymer concentrate in a uniform pelletized form. PolyS.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa JH830T Flame Retardant PC Features:UL V-0 @ 2.4mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceTransparentApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInfor.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PA6-RG30 Flame Retardant, 30% Glass Fiber Reinforced PA6 Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesApplications:Injection moldingConnectorsRelayBobbinsPlugsInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Kingfa PA6-T25 25% Mineral Filled PA6 Features:Low tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
DuPont™ Appeel® 20D855 Ethylene Acrylate DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
DuPont™ Fusabond® P613 Polymer Modifier DuPont™ Fusabond® P613 is a anhydride modified polypropylene. FUSABOND P613 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlay.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 35 BA 320 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 320 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 320 is particularly.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 35 BA 40 Copolymer Ethylene - Butyl Acrylate LOTRYL® 35 BA 40 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. Co-monomer content is 35% in weight. LOTRYL® 35 BA 40 is particularly r.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-MAX® 804 Efficiency masterbatch, PET based Fields of application: Masterbatch for improvement of production efficiency and product quality.Examples: PET cast and blown films, pipes, tubes, wire and cables, blow moulding and general extrusion.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® CL 622 Nucleation masterbatch, PP based Fields of application: Injection molded, extruded and thermoformed articles made from PP resins.Examples: Injection molded, extruded and thermoformed articles made from PP resins. Mode of action and.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® DS 785 Desiccant masterbatch in PP carrier Fields of application: Highly concentrated desiccant masterbatch for HDPE and PP.Examples: Elimination of moisture from (recycle) polymers in moisture sensitive applications.Mode of action and advan.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, .. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Addcomp ADD-VANCE® THC 453 PP based masterbatch containing heat stabilizers and carbon black Fields of application: Stabilization masterbatch for producing long fiber reinforced polypropylene for D-LFT processExamples: Long fiber reinforced pellets to be used for automotive parts, like unde.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTADER® 6200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 6200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties (reactivity, fluidity), LOTADER 62.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 14 MGC 02 Copolymer Ethylene - Methyl Acrylate LOTRYL® 14 MGC 02 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the Methyl Acrylate content, LOTRYL® 14 MGC 02 is a polymer o.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
PolyChem Alloy PolyGard 7507N PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph.. |
|||
Processing Temperature | <= 300 °C | <= 572 °F | |
Arkema Group LOTRYL® 17 BA 07 Copolymer Ethylene - Butyl Acrylate LOTRYL® 17 BA 07 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 07 is used as tie layer in coextrusion PP/PE, for extrusi.. |