Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 275 °C | 527 °F | |
Nylene® 733 Nylon 6 Dry as molded. Injection molding grade. Nylene 733 is a high impact modified nylon suitable for both molding and extrusion. Parts molded from 733 have excellent impact strength right out of the mol.. |
|||
Processing Temperature | 275 °C | 527 °F | |
Nylene® 734 Nylon 6 Dry as molded. Injection molding grade. Nylene 734 is the heat stabilized version of 733 which is a high impact modified nylon suitable for both molding and extrusion. In addition to heat stabiliza.. |
|||
Processing Temperature | 275 °C | 527 °F | |
Nylene® NX3055I Nylon 6 Dry as molded. Film Grade. Nylene NX3055I is an extrusion grade nylon 6 suitable for cast film, blown film, and co-extrusion applications. NX3055I is highly crystalline which yields excellent roll.. |
|||
Processing Temperature | 275 °C | 527 °F | |
Nylene® PX1719 Nylon 6 Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR30 30% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is.. |
|||
Processing Temperature | 275 °C | 527 °F | Typical extrusion metering zone. May be extruded up to 300°C. |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8230G HS 6% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8230G HS is a heat stabilized, 6% nylon 6 molding compound offering improved stiffness and dimensional stability in thin sections. It exhibits a combination of strength, stiffness and perfor.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8232G 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8232G is a 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resistance to creep under l.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Processing Temperature | 275 - 295 °C | 527 - 563 °F | |
Ter Hell Plastic Terez® PA 6.6 HT 7110 GF 41 FL-HF/2 Polyamide 66 Copolymer, 41% Glass Fiber Description: Partly aromatic Polyamide 6.6 Copolymer, 41% glass fiber reinforced and flame retardants.Application:Stiff molding parts with high stiffness by outstanding thermal stability, reduced w.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8331G HS Blend Impact Modified, 14% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8331G HS Blend is a 14% glass fiber reinforced, heat stabilized, polyamide 6 molding compound developed for applications requiring improved toughness in combination with a balance of strength.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8332G Impact Modified, 25% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8332G is a 25% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance of .. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8333G HI Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8333G HI is a 33% glass reinforced, impact modified polyamide 6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a balance .. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8334G Impact Modified, 40% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8334G is a heat stabilized, 40% glass fiber reinforced polyamide 6 molding compound developed for applications requiring a high level of stiffness combined with excellent impact performance. .. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® 8351 HS BK-102 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8351 HS BK-102 is a heat stabilized, pigmented black type 6 nylon graft copolymer developed for injection molding applications requiring a high level of toughness combined with a moderate fle.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR20 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 is a 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR30 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR30 is a 30% glass reinforced polyamide 6 injection molding compound. IT is also available in heat stabilized (Capron GR30 HS) and/or pigmented versions. The glass fiber reinforcement enhanc.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® GR40 40% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR40 is a 40% glass reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is also ava.. |
|||
Processing Temperature | 275 °C | 527 °F | See Materials Notes |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Processing Temperature | 275 °C | 527 °F | Extruder forward zone and adapter. |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |