Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 255 °C | 491 °F | |
Nylene® 600 Nylon 6 Dry as molded. Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacke.. |
|||
Processing Temperature | 255 °C | 491 °F | |
Nylene® 600 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 600 is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other applications include wire jacketing and centrif.. |
|||
Processing Temperature | 255 °C | 491 °F | |
Nylene® 601 Nylon 6, 50% RH, Extrusion Grade Extrusion grade. Nylene 601 is the heat stabilized version of 600 which is a general purpose, medium viscosity, extrusion grade resin used in applications such as rods, slabs, and tubing. Other app.. |
|||
Processing Temperature | <= 255 °C | <= 491 °F | |
Kingfa JH-R0G30 Flame Retardant and 30% Glass Fiber Reinforced PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood processing propertiesApplications:Injection moldingAutomobile instrument panelCD-ROM base pick-upOA device an.. |
|||
Processing Temperature | 255 - 265 °C | 491 - 509 °F | |
Zhejiang Juner 201-G20 20% Glass Fibre Reinforced Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 285 °C | 491 - 545 °F | |
Zhejiang Juner PA66-301-G20 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Framework of CoilsInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 285 °C | 491 - 545 °F | |
Zhejiang Juner PA66-301-HG30 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Connector AS PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |