Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 401, Nylon 6 Injection molding grade. Dry As Molded. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minima.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 401, Nylon 6, at 50% Relative Humidity Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 401D, Nylon 6 Injection molding grade. Dry as molded. Nylene 401D is a specially formulated nylon 6 molding resin possessing outstanding flow characteristics. Nylene 401D is ideally suited for applications requi.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 406 Nylon 6 Injection molding grade. Dry as molded. Nylene 406 is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles through rapid melt set-up. Parts molded f.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 409 Nylon 6 Dry as molded. Injection molding grade. Nylene 409 is a heat stabilized version of 406 which is a general purpose, fast cycling molding resin. Crystallization initiators provide fast molding cycles.. |
|||
Processing Temperature | 232 - 243 °C | 450 - 469 °F | At Nozzle |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Processing Temperature | 232 °C | 450 °F | |
Nylene® 603 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene 603 is a plasticized, high residual monomer resin designed for extrusion applications requiring excellent flexibility, high strength and good abrasion resist.. |
|||
Processing Temperature | 232 - 282 °C | 450 - 540 °F | Average value: 272 °C Grade Count:3 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Processing Temperature | 232 - 266 °C | 450 - 510 °F | Average value: 249 °C Grade Count:21 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Processing Temperature | 232 - 268 °C | 450 - 514 °F | Extrusion |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 251 °C Grade Count:9 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Processing Temperature | 232 - 268 °C | 450 - 514 °F | Extrusion |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 232 - 268 °C | 450 - 514 °F | Extrusion |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Processing Temperature | 232 °C | 450 °F | Film extrusion temperature |
Dow DOWLEX™ 2056 Linear Low Density Polyethylene, Heavy Duty Film Grade DOWLEX® 2056 Polyethylene resin is a premier polymer for heavy duty blown film applications. It is a low gel, high consistency polymer. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 .. |
|||
Processing Temperature | 232 - 282 °C | 450 - 540 °F | Average value: 257 °C Grade Count:5 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Processing Temperature | 232 - 270 °C | 450 - 518 °F | Average value: 250 °C Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma.. |