Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 220 °C | <= 428 °F | |
Premix Thermoplastics PRE-ELEC® ESD 5000 Polyolefin Compatible Dissipative Masterbatch, IDP Additive PRE-ELEC® ESD 5000 is a polyolefin compatible dissipative masterbatch developed for PP injection moulded products. The active substance is an IDP (inherently dissipative polymer) and it gives a per.. |
|||
Processing Temperature | <= 220 °C | <= 428 °F | |
Premix Thermoplastics PRE-ELEC® ESD 7140 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 7140 is a static dissipative thermoplastic masterbatch based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 7140 has been developed for.. |
|||
Processing Temperature | <= 220 °C | <= 428 °F | |
PolyChem Alloy PolySept 2007A PolySept products typically contain 5 – 20% of an antimicrobial agent that is compounded into a plastic resin. The result is an antimicrobial polymer concentrate in a uniform pelletized form. PolyS.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | Injection molding cylinder temperature |
LG Chemical IH830C PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | Metering Temperature, Extrusion |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Processing Temperature | 220 - 230 °C | 428 - 446 °F | C2 |
UBE 5034FDX33 Air Blown Nylon 6/66 Film Specialties: High transparencyLow neck-inNucleated typeApplications: Suitable for T-die,Water and Air blown process Processing: Shrink bags (Water) Pouch ( Air blown) Information provided by UBE. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Total HDPE SB 1359 High Density Polyethylene - Injection Stretch Blow Molding HDPE SB 1359 is a high density polyethylene with outstanding compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of packagi.. |
|||
Processing Temperature | 220 - 240 °C | 428 - 464 °F | |
Cossa Polimeri ESTALUX 5513 Methyl Methacrylate Acrylonitrile Butadiene Styrene Plastic blend that combines impact properties of ABS with the excellent transparency of PMMAInformation provided by Cossa Polimeri S.r.l. |
|||
Processing Temperature | 220 - 290 °C | 428 - 554 °F | |
E-Polymers Tekaloy® G70A4 Impact Resistance at Low Temperature PC/ABS Alloy Impact Resistance at Low TemperatureInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 5533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Processing Temperature | 220 °C | 428 °F | Gate Temperature; Extrusion |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 140V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 240W Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 °C | 428 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 4033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Processing Temperature | <= 220 °C | <= 428 °F | |
Addcomp ADD-VANCE® SA 420 Slip/anti-block additive Fields of application: Improves slip and anti-block properties of thermoplastics. It can also be used as a release agent for injection molded products.Examples: (L)LDPE, HDPE, PP, PS, HIPS, TPO, ABS.. |
|||
Processing Temperature | 220 - 270 °C | 428 - 518 °F | Resin Temperature |
Asahi Kasei Xyron® 220V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Processing Temperature | 220 - 260 °C | 428 - 500 °F | mass temperature |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |
|||
Processing Temperature | 220 °C | 428 °F | Typical extrusion metering zone. Do not exceed 238°C (460°F). |
DuPont Appeel® LSR 1181 Modified EVA Lidding Sealing Resin Appeel® 1181 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |