Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 204 - 218 °C | 400 - 425 °F | Suggested Stock |
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 - 238 °C | 400 - 460 °F | Average value: 221 °C Grade Count:6 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Processing Temperature | 204 - 274 °C | 399 - 525 °F | Average value: 238 °C Grade Count:10 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 710 Utility Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 710H Utility Black ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | Injection |
Shuman 730H White ABS Good impact strength, easy processability, good chemical resistanceInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 790 Black and Custom Colors ABS-Flame Retardant Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 810 Black Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 811 Black Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 881 Grey Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP810 Black Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 227 °C | 400 - 440 °F | |
Shuman SP880 Grey Polystyrene High Impact Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc. |
|||
Processing Temperature | 204 - 310 °C | 399 - 590 °F | Injection |
Dyna-Purge® C Purging Compound Designed for Purging Transparent ResinsGeneral Description:DYNA-PURGE C is a clear, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to purge high clarity.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109DL LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |
|||
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7032E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit.. |
|||
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7033E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.Availability: North America and Asia Pacific Featu.. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |
|||
Processing Temperature | 204 °C | 400 °F | Optimum cure is 1 hr. @ 400°F |
Armstrong A-701 Epoxy Adhesive A one-component, light gray, thixotropic, non-sag epoxy adhesive. A-701 uses an inert oxide filler that provides excellent electrical insulation properties. Features high temperature, 400°F, bond.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Processing Temperature | 204 °C | 400 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR
6080NC/BK have excellent soft touc.. |
|||
Processing Temperature | 204 - 260 °C | 399 - 500 °F | Stock Temperature |
Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Processing Temperature | 204 - 299 °C | 400 - 570 °F | Average value: 269 °C Grade Count:8 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |