Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 20.0 - 30.0 °C | 68.0 - 86.0 °F | Curing Agent Temperature |
Northstar Polymers MYP-V40A Polyurethane Filler Gel This polyurethane casting material is developed for applications that require inexpensive liquid resin filler such as encapsulation of a large electric components or puncture-free tire for low-speed.. |
|||
Processing Temperature | 20.0 - 60.0 °C | 68.0 - 140 °F | Chill Roll |
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec.. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | typically used at ambient temperature |
Elmer's Products Aron Alpha® 202 Cyanoacrylate Adhesive (Industrial Krazy Glue™) General purpose adhesive for a variety of applications. Various viscosities and gap filling properties available.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Fair.. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | typically used at ambient temperature |
Elmer's Products Aron Alpha® 432TW Cyanoacrylate Adhesive (Industrial Krazy Glue™) Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa.. |
|||
Processing Temperature | 20.0 °C | 68.0 °F | typically used at ambient temperature |
Elmer's Products Aron Alpha® 801 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Low odor, low chlorosis (bloom) when a transparent bond, appearance and strength are required.Low gap fill. Ethoxyethyl monomer. Excellent on rubber/plastic substrates. Fair on metal substrates. .. |
|||
Processing Temperature | 20.0 - 25.0 °C | 68.0 - 77.0 °F | |
BorsodChem ONGRONAT CR-30-40 MDI Isocyanate Description of product: Polymethylene-polyphenyl-isocyanate, 4,4-diphenyl-methane-diisocyanate (MDI) and mixture of its higher functionality, multi-ring oligomers.Field of application: With suitable.. |