Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 221-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 261-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance for use in wet electrical wire and cable applications. This gra.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 281-73MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9201-85 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Vyram™ 9203-54 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | |
Advanced Elastomer Systems VistaFlex® 715-B Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Processing Temperature | 175 - 240 °C | 347 - 464 °F | |
Advanced Elastomer Systems VistaFlex® 912-B Thermoplastic Rubber
(discontinued **) Description: A black super high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as .. |
|||
Processing Temperature | <= 175 °C | <= 347 °F | Maximum Junction Temperature |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Processing Temperature | 175 °C | 347 °F | Transition Temperature |
SK Chemicals SKYTHANE® T870A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 103-50 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 121-55W241 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Processing Temperature | 175 - 220 °C | 347 - 428 °F | Extrusion |
BASF Elastoblend LP 9192 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Processing Temperature | 175 - 220 °C | 347 - 428 °F | Extrusion |
BASF Elastollan S 50 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 175 - 220 °C | 347 - 428 °F | Extrusion |
BASF Elastollan S 60 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 175 - 220 °C | 347 - 428 °F | Extrusion |
BASF Elastollan SP 883 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
BASF Elastollan 560 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and a high abrasion resistance.Typical Applications: Heel top-pieces, castor tyres and parts requiri.. |
|||
Processing Temperature | 175 - 220 °C | 347 - 428 °F | Extrusion |
BASF Elastollan S 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 121-80M300 Thermoplastic Elastomer
(discontinued **) A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and good.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 241-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 281-64MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Extrusion |
BASF Elastollan B 95 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 253-50W232 Thermoplastic Vulcanizate
(discontinued **) Product Description: A hard, colorable thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and is formulated to replace thermoset ru.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | |
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo.. |
|||
Processing Temperature | 175 - 230 °C | 347 - 446 °F | Injection molding |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |