Processing Properties Metric English Comments
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Vinyloy™ 100 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Utility gradeApplications: Vinyloy 100 sheet is a fire retardant that can be used to substitute effectively for ABS and other utility grade thermoplastics.Features: Vinyloy 100 sheet is a recycled g..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Vinyloy™ 102 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Recycled capped FR sheetApplications: Vinyloy 102 sheet is capped sheet that can be used to substitute effectively for ABS and other grades of thermoplastic sheet for your thermoforming needs.Featur..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
KYDEX® V Acrylic/PC Thermoplastic Sheet
Utility sheetApplications: Can be used to substitute effectively for utility grade thermoplastics. It is very appropriate for hidden parts and painted parts and/or where fire retardancy is not requ..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 101 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Thermoplastic sheet for signageApplications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirableFeatures: Kydex 101 is more rigid than most o..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may..
Processing Temperature 162 - 200 °C
324 - 392 °F
Forming Temperature
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd..