Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 132 - 149 °C @Thickness 12.7 mm |
270 - 300 °F @Thickness 0.500 in |
Compression Molding |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |
|||
Processing Temperature | 132 - 166 °C | 270 - 330 °F | Mold Temperature |
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention .. |
|||
Processing Temperature | 132 - 157 °C | 270 - 315 °F | Compression Molding |
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures... |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Processing Temperature | 132 - 149 °C @Thickness 12.7 mm |
270 - 300 °F @Thickness 0.500 in |
Compression Molding |
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC QC-8700 is a vinyl ester engineered structural composite molding compound for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested f.. |
|||
Processing Temperature | 132 - 160 °C @Thickness 12.7 mm |
270 - 320 °F @Thickness 0.500 in |
Compression Molding |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8800 63% Glass Fiber Vinyl Ester SMC QC-8800 is a vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and is suggested for ap.. |
|||
Processing Temperature | 132 - 149 °C @Thickness 12.7 mm |
270 - 300 °F @Thickness 0.500 in |
Compression Molding |
Quantum Composites QC-8816 66% Glass Fiber Reinforced Polyester Hybrid SMC QC-8816 is a polyester hybrid engineered structural composite molding compound reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness and fatigue resist.. |
|||
Processing Temperature | 132 - 149 °C @Thickness 12.7 mm |
270 - 300 °F @Thickness 0.500 in |
Compression Molding |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Processing Temperature | 132 - 160 °C | 270 - 320 °F | Mold temperature |
Quantum Composites QC-2130 Phenolic 25% Glass Fiber SMC
(discontinued **) QC-2130 is a glass-reinforced sheet molding compound based on a phenolic resin matrix. It exhibits outstanding low flammability characteristics. QC-2130 is recommended for applications such as air.. |
|||
Processing Temperature | 132 - 160 °C | 270 - 320 °F | Mold temperature |
Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
(discontinued **) QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use .. |
|||
Processing Temperature | 132 - 157 °C | 270 - 315 °F | Mold temperature |
Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC
(discontinued **) QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It of.. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-7810 55% Glass Fiber Polyester SMC
(discontinued **) QC-7810 is a toughened thermoset polyester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and flame resistance. It is suggested.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1120 Prime AntiFog OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1200 Utility Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1500 Freezer Modified OPS
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC
(discontinued **) QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st.. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8704 63% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8704 is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8704FR 63% Glass Fiber Flame Retardant Vinyl Ester SMC
(discontinued **) QC-8704FR is a vinyl ester-based epoxy sheet molding compound (SMC) designed for compression and transfer molding of components requiring high structural strength. It exhibits unusual toughness, an.. |
|||
Processing Temperature | 132 - 154 °C | 270 - 310 °F | Thermoforming Temp |
Alcoa KAMA 1100 Prime Clear OPS, Sheet
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Processing Temperature | 132 - 149 °C | 270 - 300 °F | Mold temperature |
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8805 is a vinyl ester-based sheet molding compound (SMC) reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness, and fatigue resistance in the fiber .. |