Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,.. |
|||
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |
|||
Processing Temperature | 127 - 154 °C | 260 - 310 °F | Compression Molding |
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3000 High Impact Polystyrene (HIPS)
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3210 Hi-Gloss Coextruded High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3300 Very High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA AgriHIPS 3500 AgriHIPS
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Average value: 143 °C Grade Count:7 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Processing Temperature | 127 - 160 °C | 261 - 320 °F | Mold temperature |
Quantum Composites QC-8100 60% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8100 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength and corrosion resistance. Form and Colors = Rolled Shee.. |
|||
Processing Temperature | 127 °C | 260 °F | Lower Process Limit |
Spartech Polypedic A Low Density Polyethylene Description: Flexible, lower processing temperature, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOsInformation provided by Spartech. |
|||
Processing Temperature | 127 °C | 260 °F | Lower Process Limit |
Spartech Polypedic F High Density Polyethylene Description: More rigid, tough, able to withstand cold temperature applicationApplications: Neck brace; splintsInformation provided by Spartech. |
|||
Processing Temperature | 127 °C | 260 °F | Lower Process Limit |
Spartech Polypedic Modified Low Density Polyethylene Description: Flexible, wider window for forming, softApplications: Anterior shells for AFOs and KAFOs; TLSOs; passive types of HOs, WHOs and EWHOs; prosthetic flexible socketsInformation provided by.. |
|||
Processing Temperature | <= 127 °C | <= 260 °F | Upper stability limit |
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materials.ChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and.. |
|||
Processing Temperature | <= 127 °C | <= 260 °F | Upper stability limit |
AdvanSource Biomaterials ChronoPrene™ 40A Thermoplastic Rubber Elastomer ChronoPrene™ is a family of biocompatible thermoplastic elastomeric materialsChronoPrene™ is a family of easy molding, high flow rubber, with excellent chemical resistance to alcohols, acids, and .. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3100 Utility HIPS
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3200 Prime High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone trea.. |
|||
Processing Temperature | 127 - 166 °C | 260 - 330 °F | Thermoforming Temp |
Alcoa KAMA 3202 Freezer Modified High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableColors availa.. |