Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 1029 °C | 1885 °F | fusing temperature |
Wall Colmonoy COLMONOY® 56 Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides Description and Application: Contains wear-resistant chromium borides and carbides. Between Colmonoy Nos. 6 and 5 in chemistry and hardness. Better ductility and impact resistance than No. 6. For.. |
|||
Processing Temperature | 1029 °C | 1885 °F | heated for 30 min, then quenched in air and tempered 2 + 2 h at 1190°F (hardness = 45 HRC) |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |