Thermal Properties Metric English Comments
Specific Heat Capacity 1.86 J/g-°C

@Temperature 180 °C
0.445 BTU/lb-°F

@Temperature 356 °F
DSC
Eastman Eastar 5445 PCTG Copolyester, Injection Molded  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Specific Heat Capacity 1.86 J/g-°C

@Temperature 180 °C
0.445 BTU/lb-°F

@Temperature 356 °F
DSC
Eastman Eastar 5445 PCTG Copolyester, Film  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..