Polymer Property : Specific Heat Capacity = 0.280 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 1.17 J/g-°C

@Temperature 50.0 °C
0.280 BTU/lb-°F

@Temperature 122 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Specific Heat Capacity 1.17 J/g-°C

@Temperature 50.0 °C
0.280 BTU/lb-°F

@Temperature 122 °F
ASTM C351
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
Specific Heat Capacity 1.17 J/g-°C

@Temperature 500 °C
0.280 BTU/lb-°F

@Temperature 932 °F
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..
Specific Heat Capacity 1.17 J/g-°C

@Temperature 500 °C
0.280 BTU/lb-°F

@Temperature 932 °F
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber
Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus..