Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.974 J/g-°C @Temperature 100 °C |
0.233 BTU/lb-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Specific Heat Capacity | 0.975 J/g-°C @Temperature 580.0 °C |
0.233 BTU/lb-°F @Temperature 1076 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |
|||
Specific Heat Capacity | 0.974 J/g-°C @Temperature 100 °C |
0.233 BTU/lb-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |
|||
Specific Heat Capacity | 0.974 J/g-°C @Temperature 100 °C |
0.233 BTU/lb-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |
|||
Specific Heat Capacity | 0.974 J/g-°C @Temperature 100 °C |
0.233 BTU/lb-°F @Temperature 212 °F |
|
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application.. |