Specific Heat Capacity 0.910 J/g-°C

@Temperature 700 °C
0.217 BTU/lb-°F

@Temperature 1290 °F
International Mold Steel Daido DRM2 Matrix High-Speed Steel
This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t..
Specific Heat Capacity 0.910 J/g-°C

@Temperature 100 °C
0.217 BTU/lb-°F

@Temperature 212 °F
Solvay Chemicals Perchloroethylene
Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay