Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.669 J/g-°C @Temperature 500 °C |
0.160 BTU/lb-°F @Temperature 932 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
Specific Heat Capacity | 0.670 J/g-°C @Temperature 25.0 °C |
0.160 BTU/lb-°F @Temperature 77.0 °F |
|
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |