Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.530 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 600 °C |
0.127 BTU/lb-°F @Temperature 1110 °F |
|
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 400 °C |
0.127 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.530 J/g-°C @Temperature 500 °C |
0.127 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |