Polymer Property : Specific Heat Capacity = 0.123 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, GTAW, aged 4000 hours at 450°C (800°F), notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, SMAW
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, GMAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.514 J/g-°C

@Temperature 600 °C
0.123 BTU/lb-°F

@Temperature 1110 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, GTAW
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..