Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 12.7-50.8 mm thick bar, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet, aged 100 hours at 500°C HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Specific Heat Capacity | 0.461 J/g-°C @Temperature 500 °C |
0.110 BTU/lb-°F @Temperature 932 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 0.000 - 100 °C |
0.110 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 20.0 °C |
0.110 BTU/lb-°F @Temperature 68.0 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, 6.4-19.1 mm thick plate, solution heat treated HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Specific Heat Capacity | 0.460 J/g-°C @Temperature 300 °C |
0.110 BTU/lb-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |