Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.18 J/g-°C @Temperature 93.3 °C |
0.520 BTU/lb-°F @Temperature 200 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Specific Heat Capacity | 2.18 J/g-°C @Temperature 65.6 °C |
0.520 BTU/lb-°F @Temperature 150 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Specific Heat Capacity | 2.18 J/g-°C @Temperature 240 °C |
0.521 BTU/lb-°F @Temperature 464 °F |
|
Eastman Eastar AN004 Natural PCTA Copolyester EASTAR AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exp.. |
|||
Specific Heat Capacity | 2.18 J/g-°C @Temperature 100 °C |
0.520 BTU/lb-°F @Temperature 212 °F |
|
ChevronTexaco 46 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |
|||
Specific Heat Capacity | 2.18 J/g-°C @Temperature 100 °C |
0.520 BTU/lb-°F @Temperature 212 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Specific Heat Capacity | 2.18 J/g-°C @Temperature 37.8 °C |
0.520 BTU/lb-°F @Temperature 100 °F |
|
Duratherm LT Paraffinic Heat Transfer Fluid Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat.. |