Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.15 J/g-°C @Temperature 200 °C |
0.514 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire PEEK is produced to the highest industry standards and is characteriz.. |
|||
Specific Heat Capacity | 2.15 J/g-°C @Temperature 200 °C |
0.514 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Specific Heat Capacity | 2.15 J/g-°C @Temperature 200 °C |
0.514 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |