Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.95 J/g-°C @Temperature 200 °C |
0.466 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Specific Heat Capacity | 1.95 J/g-°C @Temperature 200 °C |
0.466 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Specific Heat Capacity | 1.95 J/g-°C @Temperature 200 °C |
0.466 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Specific Heat Capacity | 1.95 J/g-°C @Temperature 200 °C |
0.466 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Specific Heat Capacity | 1.95 J/g-°C @Temperature 40.0 °C |
0.467 BTU/lb-°F @Temperature 104 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |