Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.84 J/g-°C @Temperature -17.8 °C |
0.440 BTU/lb-°F @Temperature 0.000 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature -17.8 °C |
0.440 BTU/lb-°F @Temperature 0.000 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 200 °C |
0.440 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK)
(Unverified Data**) Ketaspire KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and exte.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 200 °C |
0.440 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-820 SL30 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL30 is a polyetheretherketone (PEEK) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and .. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 150 °C |
0.440 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 150 °C |
0.440 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 150 °C |
0.440 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 150 °C |
0.440 BTU/lb-°F @Temperature 302 °F |
DSC |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 20.0 °C |
0.440 BTU/lb-°F @Temperature 68.0 °F |
|
Dow SPECFLEX™ NC 630 Polyol SPECFLEX™ NC 630 polyol is a high functionality capped polyol. Its high molecular weight and primary hydroxyl content make it well suited for high resilience, flexible molded foams. CAS# 009082.. |
|||
Specific Heat Capacity | 1.84 J/g-°C @Temperature 20.0 °C |
0.440 BTU/lb-°F @Temperature 68.0 °F |
|
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt.. |