Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.72 J/g-°C @Temperature 600 °C |
0.411 BTU/lb-°F @Temperature 1110 °F |
|
Zoltek Panex 35® Carbon Felt Carbon FeltApplications include: Thermal, Corrosive, or Conductive applications |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 100 °C |
0.410 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 100 °C |
0.410 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 100 °C |
0.410 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 100 °C |
0.410 BTU/lb-°F @Temperature 212 °F |
DSC |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 60.0 °C |
0.410 BTU/lb-°F @Temperature 140 °F |
DSC |
Eastman Tritan FX100 Copolyester Eastman Tritan FX100 is an amorphous copolyester that combines clarity and toughness with heat and chemical resistance. Films manufactured from this new-generation copolyester can be thermoformed w.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 60.0 °C |
0.410 BTU/lb-°F @Temperature 140 °F |
DSC |
Eastman Tritan MP100 Copolyester Eastman Tritan MP100 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation co.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 200 °C |
0.410 BTU/lb-°F @Temperature 392 °F |
ASTM E1269 |
DAK Americas Laser+® MB912 PET Product Description: Laser+® MB912 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. It delivers fast, efficient pr.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 60.0 °C |
0.411 BTU/lb-°F @Temperature 140 °F |
|
Dow SPECFLEX™ NC 700 Polyol SPECFLEX™ NC 700 polyol is a unique grafted polyether polyol containing copolymerized styrene and acrylonitrile. It is manufactured without the use of BHT and has been filtered to 200 microns. CA.. |
|||
Specific Heat Capacity | 1.72 J/g-°C @Temperature 100 °C |
0.411 BTU/lb-°F @Temperature 212 °F |
|
Dow VORANATE™ T-80 toluene diisocyanate (TDI) VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexib.. |