Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.28 J/g-°C @Temperature 50.0 °C |
0.306 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Specific Heat Capacity | 1.28 J/g-°C @Temperature 50.0 °C |
0.306 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Specific Heat Capacity | 1.28 J/g-°C @Temperature 50.0 °C |
0.306 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining.. |
|||
Specific Heat Capacity | 1.28 J/g-°C @Temperature 50.0 °C |
0.306 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |