Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.700 J/g-°C @Temperature 100 - 200 °C |
0.167 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Rocar® SiF Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 20.0 °C |
0.167 BTU/lb-°F @Temperature 68.0 °F |
DINV ENV 821-3 |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 25.0 °C |
0.167 BTU/lb-°F @Temperature 77.0 °F |
|
COI Ceramics Nicalon™ HI Type S SiC Ceramic Fiber Description: A stoichiometric beta-SiC fiber manufactured near-oxygen-free using decarbonization pyrolysis and electron-beam curing. It has higher modulus, creep resistance and oxidation resistance .. |
|||
Specific Heat Capacity | 0.700 J/g-°C @Temperature 538 °C |
0.167 BTU/lb-°F @Temperature 1000 °F |
|
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |